Análisis comparativo de la densidad y la resistencia a compresión del hormigón celular elaborado con agente espumante frente al hormigón tradicional
| dc.contributor.advisor | Navarro Peñaherrera Carlos Patricio | |
| dc.contributor.author | Moreno Meza Valeria Estefania | |
| dc.contributor.editor | Universidad Técnica de Ambato-Facultad de Ingeniería Civil y Mecánica-Carrera de Ingeniería Civil | |
| dc.date.accessioned | 2026-01-28T15:45:32Z | |
| dc.date.issued | 2026-01-28 | |
| dc.description | El presente trabajo desarrolla un análisis comparativo entre el hormigón celular elaborado con diferentes porcentajes de agente espumante (1%, 2%, 3%, 4% y 5%) frente al hormigón tradicional, con la finalidad de evaluar la densidad, resistencia a compresión y costos. La investigación se desarrolla con la necesidad de reducir el peso del hormigón, optimizando los áridos para así reducir el impacto ambiental y económico, ya que la densidad aumenta el consumo de agregados y por ende aumenta el costo en obra. La metodología se llevó a cabo en tres fases: caracterización de agregados pétreos y dosificación usando el método de la ACI 211.1, continuando con la fabricación y curado de las probetas en base a la norma NTE INEN 1573 y 1576 y finalmente el análisis de resultados obtenidos. Las probetas cilíndricas elaboradas fueros de (100x200 mm, tres para cada porcentaje espumante y sus propiedades fueron analizadas para todas las edades, se realizó mediciones de densidad y resistencia a compresión, tomando el promedio de las tres probetas. Los resultados muestran una reducción de la densidad al incorporar el agente espumante, sin embargo, no es de forma lineal. El hormigón tradicional presentó los valores más altos de densidad, alcanzando hasta 2310.5 kg/m3 a los 14 días, mientras que el hormigón celular más liviano fuel el de la mezcla del 3% con un valor de 2251.7 kg/m3 a los 28 días. En cuanto a la resistencia, el porcentaje óptimo igual fue del 3%, alcanzando una resistencia de 255.95 kg/cm2 a los 28 días, superando así al hormigón tradicional que solo obtuvo un valor de 213.12 kg/cm2 , los demás porcentajes presentaron resistencias menores, pero igual superando al hormigón tradicional, algo que hay que recalcar es que a medida que sube el porcentaje de espumante se genera mayor porosidad y su resistencia baja, el porcentaje del 3% aumentó un 21% frente al hormigón tradicional. El análisis de costos reflejó una reducción progresiva a medida que aumenta el porcentaje de espumante, el mayor costo es del hormigón tradicional con 138.87 USD/m3, mientras que el menor fue del 5% con 137.63 USD/m3 En conclusión, el hormigón celular con un porcentaje del 3% de agente espumante fue el óptimo, este posee una menor densidad combinado con el aumento de resistencia y es más económico que el hormigón tradicional. | |
| dc.description.abstract | The present work develops a comparative analysis between cellular concrete produced with different percentages of foaming agent (1%, 2%, 3%, 4%, and 5%) and traditional concrete, with the purpose of evaluating density, compressive strength, and costs. The study arises from the need to reduce the weight of concrete, optimizing aggregates to decrease environmental and economic impacts, since higher density increases aggregate consumption and consequently raises construction costs. The methodology was carried out in three phases: characterization of aggregates and mix design using the ACI 211.1 method, followed by the fabrication and curing of the specimens based on NTE INEN 1573 and 1576 standards, and finally the analysis of the obtained results. Cylindrical specimens (100×200 mm) were prepared—three for each foaming percentage—and their properties were evaluated at all curing ages. Measurements of density and compressive strength were performed, taking the average of the three specimens. The results show a reduction in density when incorporating the foaming agent; however, this behavior is not linear. Traditional concrete exhibited the highest density values, reaching up to 2310.5 kg/m³ at 14 days, while the lightest cellular concrete mix was the 3% formulation, with a density of 2251.4 kg/m³ at 21 days. Regarding compressive strength, the optimal percentage was also 3%, achieving a strength of 255.95 kg/cm² at 28 days, surpassing traditional concrete, which reached only 213.12 kg/cm². The other mixes exhibited lower strengths, although still exceeding the traditional concrete. It is important to highlight that as the percentage of foaming agent increases, porosity rises and strength decreases; the 3% mix increased its strength by 21% compared to traditional concrete. The cost analysis revealed a progressive reduction as the foaming agent percentage increased. Traditional concrete showed the highest cost at 138.87 USD/m³, while the lowest cost corresponded to the 5% mix, at 137.63 USD/m³. In conclusion, cellular concrete with 3% foaming agent was the optimal mixture, as it achieved lower density combined with higher strength and was more economical than traditional concrete. | |
| dc.identifier.citation | Universidad Técnica de Ambato-Facultad de Ingeniería Civil y Mecánica-Carrera de Ingeniería Civil | |
| dc.identifier.uri | https://repositorio.uta.edu.ec/handle/123456789/46539 | |
| dc.language.iso | es | |
| dc.publisher | Universidad Técnica de Ambato-Facultad de Ingeniería Civil y Mecánica-Carrera de Ingeniería Civil | |
| dc.subject | HORMIGÓN CELULAR | |
| dc.subject | HORMIGÓN TRADICIONAL | |
| dc.subject | AGENTE ESPUMANTE | |
| dc.subject | DENSIDAD DEL HORMIGÓN | |
| dc.title | Análisis comparativo de la densidad y la resistencia a compresión del hormigón celular elaborado con agente espumante frente al hormigón tradicional | |
| dc.type | bachelorThesis |
Archivos
Bloque original
1 - 1 de 1
Cargando...
- Nombre:
- Tesis I.C 2118 Moreno Meza Valeria Estefania.pdf
- Tamaño:
- 3,38 MB
- Formato:
- Adobe Portable Document Format
Bloque de licencias
1 - 1 de 1
Cargando...
- Nombre:
- license.txt
- Tamaño:
- 1,71 KB
- Formato:
- Item-specific license agreed upon to submission
- Descripción: