Análisis comparativo de la resistencia a la compresión de un hormigón tradicional y un hormigón con sustitución del agregado fino por arcilla al 5% y 10% en volumen

dc.contributor.advisorNavarro Peñaherrera Carlos Patricio
dc.contributor.authorFlores Tipan Danny Vladimir
dc.contributor.editorUniversidad Técnica de Ambato-Facultad de Ingeniería Civil y Mecánica-Carrera de Ingeniería Civil
dc.date.accessioned2026-07-01T19:05:03Z
dc.date.issued2026-07-01
dc.descriptionEl presente trabajo experimental se enfocó en el análisis comparativo de la resistencia a compresión de un hormigón tradicional y un hormigón con sustitución del agregado fino por arcilla al 5% y 10% en volumen, con el propósito de efectuar una evaluación profunda de las propiedades mecánicas, con el objetivo de determinar si la sustitución del material mencionado es una opción factible para potenciar el desempeño a compresión delhormigón, impulsando la eficiencia de recursos y la responsabilidad ecológica de la industria. Se diseñaron tres mezclas mediante el método ACI 211.1 para una resistencia objetivo de 240 kg/cm2, una muestra patrón 0% arcilla, una con 5% y otra con 10% de sustitución. Se elaboraron 36 probetas cilíndricas ensayadas a los 7, 14, 21 y 28 días bajo la norma NTE INEN 1573. Los resultados a los 28 días determinaron que el hormigón patrón supero el diseño alcanzando 263.77 kg/cm2. En contraste, la mezcla con 5% de arcilla obtuvo 237.08 kg/cm2 reducción del 10.1% y la de 10% alcanzo 232.16 kg/cm2 reducción del 12.0%. no logrando ninguna de las dos dosificaciones alternativas la resistencia estructural requerida. La disminución mecánica se atribuye a la alta demanda de agua de la arcilla, debilitando a la adherencia en la zona de transición interfacial. Losresultados experimentales determinan que la sustitución de agregado fino por el material de reemplazo reduce la resistencia a la compresión. Por lo tanto, se descarta su uso para hormigones estructurales de 240 kg/cm2, e valuar menos porcentajes o aplicaciones en elementos no estructurales.
dc.description.abstractThis experimental study focused on a comparative analysis of the compressive strength of traditional concrete and concrete in which the fine aggregate was replaced with clay at 5% and 10% by volume, with the aim of conducting a thoro evaluation of the mechanical properties to determine whether replacing the fine aggregate with clay is a feasible option for enhancing the compressive performance of concrete, thereby promoting resource efficiency and environmental responsibility in the industry. Three mixtures were designed using the ACI 2111.1 method for a target strength of 240 kg/cm², including a control sample with 0% clay, one with 5% substitution, and another with 10% substitution. Thirty-six cylindrical specimens were cast and tested at 7, 14, 21, and 28 days in accordance with NTE INEN 1573. The results at 28 days showed that the control concrete exceeded the design strength, reaching 263.77 kg/cm². In contrast, the mixture with 5% clay achieved 237.08 kg/cm², a reductionof 10.1%, and the one with 10% reached 232.16 kg/cm², a reductionof 12.0%. Neither of the two alternative dosages achieved the required structural strength. The decrease in mechanical strength is attributed to the high water demand of the clay, which weakens adhesion in the interfacial transition zone. The experimental results show that replacing fine aggregate with the substitute material reduces compressive strength. Therefore, its use is ruled out for structural concrete with a compressive strength of 240 kg/cm², and lower replacement ratios or its use in non-structural elements should be considered.
dc.identifier.citationUniversidad Técnica de Ambato-Facultad de Ingeniería Civil y Mecánica-Carrera de Ingeniería Civil
dc.identifier.urihttps://repositorio.uta.edu.ec/handle/123456789/46919
dc.language.isoes
dc.publisherUniversidad Técnica de Ambato-Facultad de Ingeniería Civil y Mecánica-Carrera de Ingeniería Civil
dc.subjectARCILLA
dc.subjectCOMPRESIÓN
dc.subjectDOSIFICACIÓN
dc.subjectRESISTENCIA
dc.subjectDISEÑO DE HORMIGON.
dc.titleAnálisis comparativo de la resistencia a la compresión de un hormigón tradicional y un hormigón con sustitución del agregado fino por arcilla al 5% y 10% en volumen
dc.typebachelorThesis

Archivos

Bloque original

Mostrando 1 - 1 de 1
Cargando...
Miniatura
Nombre:
Tesis I.C 2144 Flores Tipan Danny Vladimir.pdf
Tamaño:
19,35 MB
Formato:
Adobe Portable Document Format

Bloque de licencias

Mostrando 1 - 1 de 1
Cargando...
Miniatura
Nombre:
license.txt
Tamaño:
1,71 KB
Formato:
Item-specific license agreed upon to submission
Descripción: