Influencia del polvo de lijado y viruta de cuero en las propiedades mecánicas y de retracción por fraguado en morteros de cemento hidráulico
| dc.contributor.advisor | Ramírez Cabrera Wladimir José | |
| dc.contributor.author | Analuisa Lalaleo Richard David | |
| dc.contributor.editor | Universidad Técnica de Ambato-Facultad de Ingeniería Civil y Mecánica-Carrera de Ingeniería Civil | |
| dc.date.accessioned | 2026-01-28T16:01:43Z | |
| dc.date.issued | 2026-01-28 | |
| dc.description | La presente investigación evalúa la influencia del polvo de lijado de cuero (BD) y la viruta de cuero (CS), residuos generados en la industria de la curtición de cuero, en las propiedades mecánicas y el comportamiento frente a la retracción por fraguado de morteros de cemento hidráulico. El estudio surge como alternativa técnica y ambiental ante la elevada generación de residuos sólidos de la industria del cuero y la necesidad de materiales más sostenibles en la construcción. La metodología se estructuró en tres fases principales: (i) caracterización fisicoquímica de ambos residuos, determinándose altos contenidos de materia orgánica, nitrógeno y cromo total; (ii) evaluación granulométrica, absorción y dosificación de morteros; y (iii) análisis de desempeño mecánico a compresión, flexión y tracción indirecta, así como el comportamiento frente al agrietamiento por retracción plástica. Los resultados evidenciaron comportamientos opuestos entre los dos residuos. La incorporación de CS como adición logró mejoras mecánicas a bajas dosificaciones. Con 1 kg/m³, la resistencia a compresión aumentó un 23 %, la flexión un 39.5 % y la tracción un 24 %, respecto al mortero control. Así mismo, el CS redujo significativamente el agrietamiento plástico, con disminuciones en la longitud de fisuras entre 33 % y 80 % dependiendo de la dosis, destacándose 10 kg/m³ como la dosificación más eficaz en mitigación. El mecanismo dominante fue el puenteo de fisuras y el refuerzo fibroso en estado plástico y endurecido. Por el contrario, el reemplazo parcial de arena por BD produjo reducciones severas en todas las propiedades mecánicas: pérdidas entre el 75 % a 97 % en compresión, 81 % a 98.5 % en flexión y 63 % a 96 % en tracción. Su muy baja densidad aparente, alta absorción de agua y morfología generaron matrices porosas, pérdida del esqueleto granular y baja adherencia pasta–partícula. Además, el BD incrementó la carga orgánica del mortero y fue el residuo que mayor cromo aportó; incluso tras la inmovilización cementicia, en varios casos superó el límite TCLP, señalándolo como un material inviable para su uso en morteros de revoque en su estado base. Las conclusiones del estudio indican que la hipótesis es válida para CS, pero se rechaza para BD. El CS, empleado en bajas dosis, mejora el desempeño mecánico y controla el agrietamiento temprano sin comprometer la estabilidad química. En cambio, el BD no resulta adecuado como reemplazo de árido fino, pues afecta negativamente la resistencia, la microestructura y la seguridad ambiental del mortero. | |
| dc.description.abstract | This research evaluates the influence of leather buffing dust (BD) and chrome shaving waste (CS), residues generated by the leather tanning industry, on the mechanical properties and earlyage shrinkage behavior of hydraulic cement mortars. The study emerges as a technical and environmental alternative to the high generation of solid waste from the leather industry and the growing need for more sustainable construction materials. The methodology was structured into three main phases: (i) physicochemical characterization of both residues, which revealed high contents of organic matter, nitrogen, and total chromium; (ii) particle size analysis, water absorption assessment, and mortar mix design; and (iii) mechanical performance analysis through compressive, flexural, and indirect tensile strength tests, as well as the evaluation of plastic shrinkage cracking behavior. The results showed opposing behaviors between the two residues. The incorporation of CS as an additive improved mechanical performance at low dosages. At 1 kg/m³, compressive strength increased by 23%, flexural strength by 39.5%, and tensile strength by 24% compared with the control mortar. Likewise, CS significantly reduced plastic cracking, decreasing crack length between 33% and 80%, depending on the dosage, with 10 kg/m³ identified as the most effective formulation for crack mitigation. The dominant mechanism was crack-bridging and fibrous reinforcement in both the plastic and hardened states. In contrast, the partial replacement of sand with BD resulted in severe reductions in all mechanical properties: losses ranged from 75% to 97% in compressive strength, 81% to 98.5% in flexural strength, and 63% to 96% in tensile strength. It’s very low bulk density, high water absorption, and morphology produced porous matrices, loss of granular skeleton, and poor paste–particle adhesion. Additionally, BD increased the organic load of the mortar and contributed the highest chromium content; even after cementitious immobilization, several mixes exceeded the TCLP limit, identifying BD as an unfeasible material for use in plastering mortars in its raw state. The findings indicate that the research hypothesis is validated for CS but rejected for BD. CS, used at low dosages, enhances mechanical performance and controls early-age cracking without compromising chemical stability. Conversely, BD is not suitable as a fine aggregate replacement, as it negatively affects strength, microstructure, and environmental safety of the mortar. | |
| dc.identifier.citation | Universidad Técnica de Ambato-Facultad de Ingeniería Civil y Mecánica-Carrera de Ingeniería Civil | |
| dc.identifier.uri | https://repositorio.uta.edu.ec/handle/123456789/46547 | |
| dc.language.iso | es | |
| dc.publisher | Universidad Técnica de Ambato-Facultad de Ingeniería Civil y Mecánica-Carrera de Ingeniería Civil | |
| dc.subject | MORTERO | |
| dc.subject | VIRUTA DE CUERO | |
| dc.subject | POLVO DE LIJADO | |
| dc.title | Influencia del polvo de lijado y viruta de cuero en las propiedades mecánicas y de retracción por fraguado en morteros de cemento hidráulico | |
| dc.type | bachelorThesis |
Archivos
Bloque original
1 - 1 de 1
Cargando...
- Nombre:
- Tesis I.C 2120 Analuisa Lalaleo Richard David.pdf
- Tamaño:
- 8,84 MB
- Formato:
- Adobe Portable Document Format
Bloque de licencias
1 - 1 de 1
Cargando...
- Nombre:
- license.txt
- Tamaño:
- 1,71 KB
- Formato:
- Item-specific license agreed upon to submission
- Descripción: