    Análisis de la dureza y resistencia al desgaste de materiales poliméricos comerciales utilizados en componentes mecánicos
    (Universidad Técnica de Ambato-Facultad de Ingeniería Civil y Mecánica-Carrera de Ingeniería Mecánica, 2026-07-06)
    Cando Chicaiza Israel Vladimir
    ;
    Vaca Ortega Wilson Henry
    ;
    Universidad Técnica de Ambato-Facultad de Ingeniería Civil y Mecánica-Carrera de Ingeniería Mecánica
    This research paper characterizes and evaluates the mechanical and tribological behavior of four commercial engineering polymers Duralon, Grilon, Nylon, and Teflon commonly implemented in the manufacturing of industrial mechanical components. The experimental phase was executed under standardized protocols, conducting indentation hardness tests utilizing a Shore Type D durometer in accordance with the ASTM D2240- 15 standard, and dynamic abrasive wear tests employing a Taber rotary mechanism according to the ISO 9352 specification. Duralon exhibited the highest structural rigidity and the lowest Taber wear index, demonstrating excellent dimensional stability under localized stresses. On the other hand, Teflon, despite registering the lowest surface hardness, achieved highly efficient wear resistance. This behavior is scientifically justified by the activation of an intrinsic molecular self-lubrication mechanism and the subsequent formation of a polymer-to-polymer transfer film on the abrasive wheels. Grilon displayed superior tribological and mechanical performance compared to standard Nylon due to its higher molecular density. Nylon exhibited the highest vulnerability to severe abrasion, driven by friction-induced thermo-mechanical plasticization and its inherent hygroscopic susceptibility. Finally, this mechanical analysis delivers structured material selection criteria for mechanical components, establishing Duralon as the optimal candidate for high structural load configurations, and designating Teflon as the primary alternative for continuous sliding interfaces where external lubrication is technically restrictive.