dc.descriptionEste trabajo experimental analiza cómo influye la aplicación de diferentes velocidades de carga, tipos de curado y tamaño de los especímenes en los valores de resistencia cilíndrica a compresión en las edades de 7, 14 y 28 días. Para ello se adquirieron los agregados de la Cantera Salvador ubicada en la ciudad de Ambato - sector Aguaján y Cemento Tipo GU para sus posteriores ensayos de caracterización de acuerdo a las normas INEN y ASTM, luego se procedió a realizar la dosificación aplicando el Método de la Densidad Óptima para un hormigón con resistencia de diseño de 210 kilogramos sobre centímetros cuadrados. Con la dosificación definitiva se elaboraron 63 especímenes para determinar sus propiedades en estado fresco y endurecido dependiendo de las variables a aplicarse en cada uno de ellos. En lo referente a los resultados obtenidos de resistencia a compresión a los 28 días, a una velocidad de 0.475 MPa/s se obtuvo un incremento del 7.07 por ciento, mientras que para una velocidad de 0.025 MPa/s se da una disminución del 5.22 por ciento de la resistencia obtenida a la velocidad normada. Por otro lado, los especímenes no sometidos a un proceso de curado alcanzan un 86.15 por ciento de la resistencia a la compresión adquirida por los especímenes que fueron curados. Finalmente, en lo que respecta al tamaño de espécimen se determinó que los de 100x200 mm adquiere un 8.88 por ciento más de resistencia que especímenes de 150x300 mm.es_ES
dc.description.abstractThis experimental work analyzes the influence of the application of different loading rates, types of curing and specimen size on the values of cylindrical compressive strength at ages 7, 14 and 28 days. For this purpose, aggregates were acquired from the Salvador Quarry located in the city of Ambato - Aguaján sector and Type GU Cement for subsequent characterization tests according to INEN and ASTM standards, then the dosage was carried out applying the Optimum Density Method for a concrete with a design strength of 210 kilograms over square centimeters. With the final dosage, 63 specimens were prepared to determine their properties in fresh and hardened state depending on the variables to be applied in each one of them. Regarding the results obtained for compressive strength at 28 days, at a speed of 0.475 MPa/s an increase of 7.07 percent was obtained, while for a speed of 0.025 MPa/s there was a decrease of 5.22 percent of the strength obtained at the standard speed. On the other hand, specimens not subjected to a curing process reach 86.15 percent of the compressive strength acquired by the specimens that were cured. Finally, with respect to specimen size, it was determined that 100x200 mm specimens acquired 8.88 percent more strength than 150x300 mm specimens.es_ES
dc.language.isospaes_ES
dc.publisherUniversidad Técnica de Ambato. Facultad de Ingeniería Civil y Mecánica, Carrera de Ingeniería Civiles_ES
dc.rightsopenAccesses_ES
dc.subjectHORMIGÓNes_ES
dc.subjectRESISTENCIA A COMPRESIÓNes_ES
dc.subjectVELOCIDAD DE CARGAes_ES
dc.subjectCURADOes_ES
dc.subjectTAMAÑO DEL ESPÉCIMENes_ES
dc.titleAnálisis de la influencia de la velocidad de carga, curado y tamaño del espécimen en la resistencia cilíndrica a compresión del hormigónes_ES
dc.typebachelorThesises_ES
Aparece en las colecciones: Ingeniería Civil

Ficheros en este ítem:
Fichero Descripción Tamaño Formato  
Tesis C.I. 1573 - Freire Ocaña Jazmina Beatriz.pdfTESIS A TEXTO COMPLETO2,45 MBAdobe PDFVisualizar/Abrir


Los ítems de DSpace están protegidos por copyright, con todos los derechos reservados, a menos que se indique lo contrario.