dc.descriptionEste trabajo experimental tiene como objetivo principal: Analizar los revestimientos duros aplicados por proceso SMAW sobre acero al carbono A36 y su incidencia en el desgaste abrasivo evaluado bajo la norma ASTM G-6, para lo cual se fabricaron probetas de 72 x 60 x 12 mm , se recubrieron con tres tipos de electrodos de la marca Indura, 10 probetas se revistieron con electrodo a base de carburos de cromo (Overlay – 62), 5 con una pasada y 5 con dos pasadas, el mismo procedimiento se lo realizó con los electrodos a base de aleaciones Martensíticas (Antifrix-450) y con los electrodos a base de aleaciones Austeníticas altas en manganeso. La máquina en la que se realizaron los ensayos de desgaste abrasivo establecen los parámetros de la norma ASTM G-65. Los ensayos de metalografía ayudaron a verificar su microestructura en cada tipo de electrodo, también se realizaron ensayos de dureza y espectrometría para obtener su porcentaje en composición química, con el fin de analizar los parámetros que brindan mejor resistencia al desgaste. Finalmente se pesaron las muestras para obtener la diferencia de masa pérdida (g) y calcular las pérdidas volumétricas en cada uno de los casos, con lo cual se pudo determinar que la menor pérdida volumétrica se obtuvo con el electro Overlay-62 con una pérdida volumétrica de 49.909mm3y 41.697 mm3con una y dos pasadas respectivamente el segundo mejor resultado fue con el electrodo Weldmang-14 con una pérdida volumétrica de 74.58 mm3 y 65.189 mm3 con una y dos pasadas respectivamente, el electrodo que no brindo buenas características para la resistencia al desgaste fue el electrodo Antifrix-450 con una pérdida de 305.548mm3 y 274.876 mm3 con una y dos pasadas respectivamente.es_ES
dc.description.abstractThis experimental work has as main objective: Analyze the hard coatings applied by the SMAW process on carbon steel A36 and its incidence in the abrasive wear evaluated under the ASTM G-6 standard, for which 72 x 60 x 12 mm specimens were manufactured , were coated with three types of Indura brand electrodes, 10 specimens were coated with chromium carbide based electrode (Overlay - 62), 5 with one pass and 5 with two passes, the same procedure was performed with the electrodes based on Martensitic alloys (Antifrix-450) and with the electrodes based on Austenitic alloys high in manganese. The machine in which the abrasive wear tests were carried out established the parameters of the ASTM G-65 standard. The metallography tests helped to verify their microstructure in each type of electrode, hardness and spectrometry tests were also carried out to obtain their percentage in chemical composition, in order to analyze the parameters that provide better resistance to wear. Finally the samples were weighed to obtain the difference of mass loss (g) and calculate the volumetric losses in each one of the cases, with which it was possible to determine that the smaller volumetric loss was obtained with the electro-Overlay-62 with a volumetric loss of 49.909mm3 and 41.697 mm3 with one and two passes respectively the second best result was with the Weldmang-14 electrode with a volumetric loss of 74.58 mm3 and 65.189 mm3with one and two passes respectively, The electrode that did not provide good characteristics for wear resistance was the Antifrix-450 electrode with a loss of 305.548mm3 and 274.876 with one and two passes respectivelyes_ES
dc.language.isospaes_ES
dc.publisherUniversidad Técnica de Ambato. Facultad de Ingeniería Civil y Mecánica. Carrera de Ingeniería Mecánicaes_ES
dc.rightsopenAccesses_ES
dc.subjectREVESTIMIENTOS DUROSes_ES
dc.subjectSOLDADURA SMAWes_ES
dc.subjectCARBONO A36es_ES
dc.subjectNORMA ASTM G-65es_ES
dc.subjectELECTRODOSes_ES
dc.subjectDESGASTEes_ES
dc.subjectMARTENSITAes_ES
dc.subjectAUSTENITAes_ES
dc.subjectCARBUROS DE CROMOes_ES
dc.titleAnálisis de revestimientos duros aplicados por proceso SMAW sobre acero al carbono A36 y su incidencia en el desgaste abrasivo evaluado bajo la norma ASTM G-65es_ES
dc.typebachelorThesises_ES
Aparece en las colecciones: Ingeniería Mecánica

Ficheros en este ítem:
Fichero Descripción Tamaño Formato  
Tesis I. M. 444 - Bautista Romero Miltón Andrés.pdfTESIS A TEXTO COMPLETO8,16 MBAdobe PDFVisualizar/Abrir


Los ítems de DSpace están protegidos por copyright, con todos los derechos reservados, a menos que se indique lo contrario.